| 性能項目 | 試驗條件[狀態] | 測試 | 測試數據 | 數據單位 | |
| 基本性能 | 熔體流動速率 | ASTM D-1238 | 30.00 | g/10min | |
| 機械性能 | 埃佐缺口沖擊強度 | -20℃ | ASTM D-256 | 4.0 | kgcm/cm2 |
| 埃佐缺口沖擊強度 | 23℃ | ASTM D-256 | 7.5 | kgcm/cm2 | |
| 彎曲彈性率 | ASTM D-790 | 14,000 | kg/cm2 | ||
| 彎曲強度 | ASTM D-790 | 370 | kg/cm2 | ||
| 斷裂伸長率 | ASTM D-638 | 200 | % | ||
| 肖氏硬度 | ASTM D-785 | 95 | R SCALE | ||
| 屈服點拉伸強度 | ASTM D-638 | 260 | kg/cm2 | ||
| 熱性能 | 熱變形溫度 | ASTM D-648 | 125 | ℃ | |
| DuPont沖擊強度 | 23℃ | ASTM HPC | 70 | kg.cm | |
| DuPont沖擊強度 | -10℃ | ASTM METHOD | 45 | kg.cm | |