| 性能項目 | 試驗條件[狀態(tài)] | 測試 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
| 基本性能 | 熔體流動速率 | 230℃ | ASTM D-1238 | 10.0 | g/10min |
| 密度 | ASTM D-1505 | 0.9 | g/cm3 | ||
| 模壓收縮率 | HPC Method | 1.50 | % | ||
| 模壓收縮率 | HPC Method | 1.50 | % | ||
| 機械性能 | Du-Pont沖擊強度 | -10℃ | HPC Method | 50 | |
| IZOD沖擊強度 | -10℃ | ASTM D-256 | 4.5 | Kg· cm/cm | |
| IZOD沖擊強度 | 23℃ | ASTM D-256 | 8.5 | Kg· cm/cm | |
| 洛氏硬度 | ASTM D-785 | 95 | R | ||
| 伸長率 | ASTM D-638 | >100 | % | ||
| 彎曲模量 | ASTM D-790 | 15,000 | Kg/cm2 | ||
| 拉伸屈服強度 | ASTM D-638 | 270 | Kg/cm2 | ||
| 熱性能 | 熱變形溫度 | 4.6MPa | ASTM D-648 | 115 | ℃ |
| 其它性能 | 阻燃性 | UL | HB | ||