TPR/TPE注塑缺陷問題解決方案:適當降低成型溫度,降低注塑速率和注射壓力,縮短注塑成型周期,并且及時清理料筒
TPR/TPE等注塑成型的制品易出現表面白化
在制品對噴嘴一側,即在頂桿位于模具頂出一側的地方出現的應力泛白的現象
外力作用是導致塑件表面白化的主要原因
TPR/TPE注塑缺陷問題解決方案:降低注射壓力,保壓壓力,縮短保壓時間,適當提高脫模斜度,特別是在加強筋和凸臺附近應防止倒退拔。脫模機構的頂出裝置要設置在塑件壁厚處或適當增加塑件頂出部位的厚度
| 產品說明Product description | ||||
| ·70S是一款高透明材料,具有良好的抗沖擊和抗疲勞性能。 ·70S is a kind of high transparent material which has excellent impact resistance and fatigue resistance properties. | ||||
| 關鍵特性Key characteristic | ||||
| 1.粘接強度非常好,可粘接材質:PS,ABS,PC Very high bonding strength,adhesive materials:PS,ABS and PC. 2.表面光亮Bright surface. 3.可噴油,絲印,上膠水,油墨Oil injection,silkscreen,can be applied with glue and ink. 4.良好的耐磨性,耐抗拉,耐撕裂性能Excellent abrasion resistance,tension resistance and tear resistance. | ||||
| 功能Function | ||||
| 產品應用 Main application | 玩具公仔Toy dolls | 泳鏡粘PC Swimming glasses PC | ||
|
| 電動牙刷Electric toothbrush |
| ||
| 加工方法Processing method | 注塑成型Injection molding | |||
| 環保認證 Environmental certification | ROHS | REACH | EN71-3 | |
|
| PAHS | ASTM-F963 | Phthalate | |
| 顏色Color | 透明Transparent | |||
| 氣味Smell | 少許樹脂味A little resin smell | |||
| 外型Appearance | 圓球形小顆粒Cylindrical particle,about 3mm×1.5mm | |||
| 儲藏期Storage period | 常溫下通風干燥,24個月Ventilated dry at normal temperature,about 24 months | |||
| 包裝方式Packaging method | 25公斤/袋 25kg/bag | |||
![]() | ![]() |
![]() | ![]() |