產品參數
| 性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | ||
| 其它性能 | 薄膜 | MD | ASTM D-638/D-882 | 480 | % | |
| TD | ASTM D-638/D-882 | 640 | % | |||
| 基本性能 | 密度 | ASTM D-1505 | g/cm3 | |||
| 機械性能 | 沖擊強度 | ASTM D-1709 | 374 | G/F50 | ||
| 其它性能 | 鑄膜成型 | ASTM D-638/D-882 | 180 | kg/cm2 | ||
| 硬度 | ASTM D-2240 | 36 | Shore D | |||
| 低溫易脆性 | ASTM D-746 | -76 | ℃/F50 | |||
| 射出 | ASTM D-638/D-882 | 250 | % | |||
| VA含量 | ASTM USIFE | 22 | % | |||
| 薄膜 | MD | ASTM D-638/D-882 | 264 | kg/cm2 | ||
| TD | ASTM D-638/D-882 | 189 | kg/cm2 | |||
| 熔融指數 | ASTM D-1238 | g/10min | ||||
| VICAT 軟化點 | ASTM D-1525 | 64 | ℃ | |||
| 融化點 | ASTM D-2117 | 82 | ℃ | |||
| 射出 | ASTM D-638/D-882 | 110 | kg/cm2 | |||
| 鑄膜成型 | ASTM D-638/D-882 | 800 | % | |||